TPO Roof Installation in Ontario: Step by Step
How a TPO roof is laid, attached and welded on a commercial building, and what to ask the contractor who installs it.
Call 1-833-775-7663 Oakville head office · TPO roofing on commercial, industrial and institutional buildings across Ontario
Karol Rajkowski
Vice President, OYH Roofing
Published October 20, 2026 · 14 min read
Short answer
TPO roof installation goes in layers: a sound, dry deck, a vapour retarder, insulation and often a cover board, then the TPO sheet, held down by screws in the seams, by adhesive or by induction-welded plates. Every seam is hot-air welded at least 38 mm (1 1/2 in) wide by machine, checked with test welds and probed the same day.
What goes under a TPO roof?
A TPO roof is one sheet of thermoplastic polyolefin, reinforced with polyester and most often 45, 60 or 80 mil thick, over the same kind of assembly as any other flat roof. Good TPO roof installation starts with those layers.
| Layer | What it does | Notes from makers, NRC and RCABC |
|---|---|---|
| TPO membrane | The waterproof top layer, usually white | 45, 60 or 80 mil, reinforced with polyester; seams hot-air welded; cut edges sealed |
| Cover board | A firm, flat surface over the insulation | High-density polyiso or gypsum; on an adhered roof, the bond to the board's facer carries the wind load (NRC) |
| Insulation | Thermal resistance, usually polyisocyanurate | Polystyrene needs a slip sheet under TPO and must not touch the adhesive (Johns Manville) |
| Vapour retarder | Keeps indoor moisture and air out of the roof | NRC tests found it raised wind uplift resistance by 25 to 50 per cent |
| Deck | The structure: steel, concrete or wood | Elevate's Canadian assemblies were tested on 22 gauge steel; RCABC does not allow an adhered membrane directly on a wood deck |
Old roofing matters too, because TPO does not mix with asphalt or coal tar: Johns Manville (U.S.) calls for a slip sheet over any asphalt roof left in place and insulation over coal tar. On the Devi Mandir temple in Pickering, we removed two layers of modified bitumen and an old coating first.
How is a TPO roof installed?
In the same order every time: approvals, deck, insulation, membrane, seams, flashings, inspection. TPO roof installation follows the maker's specification and the tested assembly chosen for the wind load, in sections that are sealed off each day. RCABC's TPO standard, cited often here, is written for B.C.'s RoofStar guarantee, but it is the most detailed Canadian TPO standard we found.
| Step | What happens | What makers and RCABC require |
|---|---|---|
| 1. Approvals and design | The maker accepts the project; a tested assembly is picked for the wind load | Elevate: no work before its Pre-Installation Notice is approved. RCABC: fasteners and plates must match the tested assembly |
| 2. Prepare the deck | Old roofing removed where needed; deck cleaned and dried | Rain, condensation, frost, snow and ice removed (IKO) |
| 3. Vapour retarder, insulation, cover board | Boards laid and fastened or glued | Only insulation approved by the membrane maker (CRCA); polystyrene kept away from the TPO (Johns Manville) |
| 4. Unroll and relax | Sheets laid flat without stretching | At least 30 minutes to relax, longer in cold weather (Elevate, IKO) |
| 5. Attach the membrane | Screws in the seams, adhesive or induction plates | Also fastened at the perimeter, at slope changes and around curbs (RCABC) |
| 6. Weld and probe the seams | Robotic welder in the field, hand welder at details | Test welds first; welds at least 38 mm by machine and 50 mm by hand; every seam probed (IKO, RCABC) |
| 7. Flashings and close-out | Walls, curbs, edges and drains finished; maker's inspection | Flashings at least 200 mm high; inspection by the maker's technical representative, not a sales representative (Elevate) |

For tear-off, daily seals and keeping a business open during the work, see our commercial roof replacement guide.
Mechanically fastened, fully adhered or induction welded?
Those are the three common ways to hold a TPO sheet down, and the building decides. CRCA's reference manual links fastened systems to flexible decks and adhered systems to unusual shapes, both where wind or fire needs are specific, and also describes loose-laid sheets under about 60 kg/m² of ballast.
| Method | How it holds | Points to watch |
|---|---|---|
| Mechanically fastened | Screws and plates along each sheet's edge, covered and welded by the next sheet's 152 mm (6 in) lap (IKO) | Rows run across the steel deck flutes (RCABC, NRC); fastener heads flush, never overdriven (IKO); welding both sides of a fastener row gave at least 15 per cent more uplift resistance than one side (NRC) |
| Fully adhered | Bonding adhesive on the board and the sheet, left to dry to the touch, then broomed or rolled in | Adhesive temperature limits; no adhesive in the lap (CRCA); solvent fumes kept out of rooftop air intakes (CRCA) |
| Induction welded | Coated plates fastened through the insulation; the underside of the sheet is welded to them, so the new membrane is not pierced | IKO's induction plates work down to -18°C if they are dry; plates at least 50 mm from laps; test welds to set the equipment (CRCA) |
In Ontario, wind is a code question. The Building Code (5.2.2.2) points to CSA A123.21 for the wind uplift resistance of membrane roofs, unless an assembly has proven past performance, and that standard tests each attachment as a complete system. Elevate's Canadian tested assemblies space fastener rows from 610 mm to 2,896 mm apart and divide every result by a safety factor of 1.5. CRCA's policy is that wind loads are set by the designer, not the roofer.
Adhered systems bring fumes. CRCA's guidance is to shut down and block rooftop air intakes while solvent adhesive goes down, work when the building is empty where possible, and restart the air only once the fumes are gone. Low-odour water-based and foam adhesives exist, but water-based ones need warm weather.
How are TPO seams welded and tested?
With hot air that melts the two sheets together. A robotic welder runs the long field seams and a hand welder does corners, walls and short runs; IKO says TPO flashings are always hand-welded. A weld cannot be judged by eye, so the checks happen every day.
- Width. At least 38 mm (1 1/2 in) with a robotic welder and 50 mm (2 in) by hand, under IKO's manual and RCABC's standard; U.S. makers use the same 1 1/2 in minimum.
- Test welds first. IKO sets each welder with test welds at the start of every workday and whenever it has been shut off. RCABC asks for a test weld daily before welding and every 2 hours after that.
- Heat and speed. IKO's typical robotic setting at 21°C and 50 per cent humidity is 510 to 570°C at 3 to 5 m a minute, adjusted through the day as conditions change. NRC warns that the wrong speed and temperature give "a very weak seam".
- Peel tests. IKO cuts 50 mm strips across finished seams in the morning, at midday and near the end of the day, and again when the weather changes. A good seam is almost impossible to peel and tears the TPO off its scrim. Each cut is then patched.
- Probing. Once the weld has cooled, a blunt probe is run along every seam. Where the probe goes in, there is a void, which is marked and repaired the same day (IKO, CRCA). Carlisle (U.S.) waits at least 30 minutes before probing.
- Power. IKO gives each robotic welder its own generator, because other tools on it cause power surges and uneven welds.
One thing not to expect is a bead of melted material along every seam. Versico (U.S.) notes that TPO does not flow like PVC; the sign it looks for is a sheen about 13 mm (1/2 in) wide on the bottom sheet, and any doubtful seam gets probed.
How are flashings, T-joints and cut edges finished?
By hand, to the maker's details. At walls and curbs the TPO turns up at least 200 mm (8 in) above the roof under IKO, Elevate and Johns Manville details, is fastened at its base with plates no more than 300 mm apart (IKO), and is hand-welded at least 50 mm wide. Metal edges are coated with TPO from the same maker so the membrane can be welded to them (CRCA, Elevate).
- T-joints. Where three layers meet, a joint cover goes over the seam. IKO requires one on 60 and 80 mil membranes, recommends it on 45 mil, and requires pre-moulded covers for its 25- and 30-year warranties.
- Cut edges. Every cut edge of reinforced TPO, factory edges included, gets a 3 mm (1/8 in) bead of the maker's cut-edge sealant (IKO, Johns Manville). IKO allows no other sealant there.
- Walkway pads. Elevate (U.S.) spaces pads 25 to 75 mm apart and adds membrane under any pad within 150 mm of a seam; RCABC puts heat-absorbing pads on a slip sheet.
- Drains and equipment. Laps stay at least 914 mm from the centre of a drain (RCABC). Curbs and units are covered in our rooftop equipment guide, and how these details fail later in our roof flashing repair guide.
Can TPO roof installation be done in winter?
Yes, within limits that depend on how the sheet is attached. IKO's cold-weather rules start below 4°C. Cold sheets are harder to lay flat, weld and glue to walls, adhesives dry more slowly, and condensation on wet adhesive, called blushing, stops it from bonding at all.
| Product or step | IKO minimum | Notes |
|---|---|---|
| Solvent membrane adhesive | 4°C, air and surface | Product kept at 15 to 27°C before use |
| Spray membrane adhesive | -4°C | Stop at once if condensation appears |
| Two-part foam insulation adhesive | 0°C | Tank kept at 21 to 29°C |
| TPO primer and sealants | -7°C | Slower drying in the cold |
| Induction welding | -18°C | No moisture or condensation on the plates |
| Membrane rolls | Stored dry, at least 4°C | Relax 30 to 60 minutes before installing |
Welding slows down too: Johns Manville (U.S.) asks for twice the usual number of peel samples below 10°C, and notes that mechanically fastened and induction-welded systems suit cold weather. IKO adds a rule worth repeating: never warm roofing materials with a torch. Our flat roofing material guide compares cold ratings for every system.
How can you tell a TPO roof was installed right?
Mostly during TPO roof installation, through test welds, peel samples and probing, because a finished seam looks the same whether it is bonded or not. The final check is the maker's inspection; Carlisle (U.S.) issues no warranty if its inspector cannot inspect the roof.
| Defect | Why it matters | Source |
|---|---|---|
| Cold or partial welds | Can pass the probe and still come apart later; IKO rejects both | FRSA, IKO |
| Scorched or overheated seams | Too much heat destroys the stabilizers in TPO; an overlay is needed even if the seam probes fine | FRSA, Versico |
| Voids, wrinkles and fishmouths in seams | Must be rewelded or cut out and patched | IKO, RCABC |
| Dirty or wet laps | Dirt, moisture or adhesive in the lap stops the weld | IKO, CRCA |
| Missing joint covers or cut-edge sealant | Required details on reinforced TPO | IKO, Johns Manville |
| Fastener rows welded on one side, or overdriven fasteners | Fasteners rock in the wind and can pull out of the steel deck | NRC, IKO |
In Canada, Elevate says each warranted project gets at least three inspections by its technical representatives, and IKO offers site visits on request. Our commercial roof warranty guide explains each warranty type.
What standards and Ontario rules apply to TPO?
A product standard for the sheet, wind and fire tests for the roof assembly, and Ontario's safety rules for the crew. None of them tells you how well a particular roof was installed.
- ASTM D6878. The specification for reinforced TPO sheet (current edition D6878/D6878M-26), covering thickness over the scrim, overall thickness and factory seam strength; it leaves the installed system out of scope. We found no CSA or CGSB standard for TPO, and RCABC accepts TPO by reference to ASTM D6878.
- CAN/ULC-S107. The fire test for roof coverings, run over a given deck and insulation, so the listed rating must match the assembly being built; see our new construction roofing guide. Wind uplift (CSA A123.21) is covered above.
- Fire Code. Ontario's Fire Code sections on hot surface applications (5.11, which includes "other heat-producing devices") and hot works (5.17, which includes adhesive bonding) do not name hot-air welding of roof membranes, so ask whether the building's own hot work rules apply.
- Flammable adhesives. Solvent-based TPO bonding adhesives are highly flammable (a flash point of -23°C on one Tremco safety data sheet), so the flammable liquid rules of O. Reg. 213/91 on storage (s. 43) and fire extinguishers (s. 52) apply.
- Electrical. The same regulation requires portable electrical tools used outdoors to be plugged into a Class A ground fault circuit interrupter (s. 195.2).
Planning a TPO roof?
We can review the deck, attachment method and details with you, and set out the membrane, thickness and warranty options for your building.
Call 1-833-775-7663Request an assessmentWhat does TPO roof repair involve?
Usually welding a new piece of TPO over the damage. CRCA's manual says thermoplastic membranes can usually be hot-air welded throughout their service life, but a TPO roof repair is only as good as the cleaning before it.
- Clean. Detergent and warm water, rinse, dry, then the maker's cleaner on a lint-free cloth, never poured onto the membrane (CRCA).
- Patch. The patch reaches 100 mm (4 in) past the damage on every side, with rounded corners. It is pre-welded about 50 mm in from its edge, the outer 50 mm is then welded, and the seam is probed once it cools (CRCA).
- Open laps. The lap is pulled back to where the bond is sound. If water got in, the membrane is opened and wet insulation replaced before the lap is rewelded and covered with a 200 mm strip (CRCA).
- Worn membrane. If the surface is too dirty or degraded to weld, CRCA enlarges the hole and welds the patch to the underside of the old sheet.
- What not to use. IKO bans oil-based or bituminous cements on its TPO, and BUILDINGS magazine (U.S.) warns that asphalt mastic on a leak means a bigger cut-out repair later and that unapproved repairs can void the warranty.
Typical repairs are open or cold-welded seams, punctures and, on fastened roofs, fasteners that rock loose and push up through the membrane (U.S. trade press). Some TPO membranes have cracked on roofs in extremely hot, sunny U.S. climates (Professional Roofing, 2015); we found no Canadian data on it. See also our membrane roof repair guide and our repair or replace guide.
How do you choose a TPO roofing contractor?
Start with the membrane maker. A TPO warranty depends on the contractor being authorized by the maker and on the maker inspecting the roof, so a TPO roofing contractor's standing with the maker matters as much as its references. For WSIB clearance, insurance and other general checks, see our guide to choosing a commercial roofing contractor.
In Canada, IKO's Approved Applicator Program asks for two years of commercial roofing experience, training and completed warranty jobs, with a Diamond level, including hands-on training, for its Diamond Shield system warranties. Elevate's licensed contractors complete its Contractor Quality Seminars. CRCA says only workers trained to the maker's specifications should weld seams.
| Question | Why it matters |
|---|---|
| Which maker, which membrane and what thickness? | Warranty terms follow thickness: IKO's Diamond Shield runs up to 15 years on 45 mil, 20 on 60 mil and 30 on 80 mil (U.S. brochure) |
| Are you authorized by that maker now, and at what level? | Ask for a current letter on the maker's letterhead (Colorado Roofing Association) |
| How will the sheet be attached, and to which tested assembly? | Fasteners and plates must match the CSA A123.21 tested assembly; RCABC says substitutions may void its guarantee |
| Will you keep test weld, peel test and probing records? | IKO and RCABC require these checks every day; records and photos show they were done |
| Who inspects the finished roof, and what warranty will we get? | A total system (no dollar limit) warranty covers materials and labour; a material-only warranty covers only failed material |
What TPO roofs has OYH Roofing installed?
OYH Roofing handles TPO roof installation on commercial, industrial and institutional buildings across Ontario. At Millomat Stampings in Mississauga, we installed one 60 mil TPO system across 50,000 sq ft, covering a new addition and a re-roof of the existing building. At the Devi Mandir temple in Pickering, we removed two layers of modified bitumen and an old coating and installed 6,500 sq ft of 60 mil TPO. Both roofs carry 20-year warranties on labour and materials.
See the Millomat Stampings project, the Devi Mandir project and our other completed projects. To compare systems first, see TPO vs EPDM, PVC vs TPO and modified bitumen vs TPO; for lifespans, see how long a commercial flat roof lasts.
Frequently asked questions
How is TPO attached to a roof?
In one of three common ways: screws and plates along the edge of each sheet, covered by the next sheet's weld (mechanically fastened); bonding adhesive under the whole sheet (fully adhered); or coated plates welded to the underside of the sheet (induction welded). CRCA also describes loose-laid sheets held down by ballast. The wind design and the deck decide which.
What temperature does TPO weld at?
It depends on the welder, the speed and the weather. IKO's typical starting point for a robotic welder at 21°C and 50 per cent humidity is 510 to 570°C at 3 to 5 m a minute, adjusted through the day. Crews confirm the setting with test welds and peel tests each morning and whenever conditions change.
Do you need seam tape for TPO?
Not for the field seams, which are hot-air welded at least 38 mm wide by machine and 50 mm by hand. Seams, joint covers and patches on a TPO roof are welded TPO, and IKO says pre-taped cover tapes should never be welded. Cut edges of reinforced sheet get a bead of the maker's cut-edge sealant instead.
Can TPO go directly on plywood?
Not as an adhered roof under RCABC's standard, which allows an adhered single-ply membrane on a wood deck only over an accepted deck overlay. On commercial roofs, TPO normally goes over insulation and a cover board, and the maker's tested assembly sets what the sheet may be fastened or glued to.
Can I install TPO myself?
Not on a commercial roof that needs a warranty. The makers we checked issue system warranties only through authorized or licensed contractors, after their own inspection, and CRCA says only workers trained to the maker's specifications should weld seams. Robotic welders, daily test welds and Ontario's fall protection rules are all part of TPO roof installation.
Need a roof that lasts?
Tell us about your building and roof, and we will set up a roof assessment and a written quote.
Call 1-833-775-7663Request an assessment
Karol Rajkowski
Vice President · OYH Roofing
Karol Rajkowski is Vice President of OYH Roofing, an Oakville-based ICI flat-roofing contractor whose projects include the 50,000 sq ft TPO roof at Millomat Stampings in Mississauga and the Marriott Hotel in Vaughan. Learn more about the OYH team.
Sources
- IKO: Innovi TPO Roofing Systems Installation Manual, Canada; Innovi TPO Cold Weather Guidelines (December 2025); details T-SM-5, T-SM-9 and T-BT-1 (2025); IKO Approved Applicator Program, Canada (September 2024); InnoviTPO system brochure (2024, U.S.).
- Holcim Elevate: UltraPly TPO tested assembly guide, CSA (July 2025); UltraPly TPO specification 07 54 23 (2023, U.S.); National Accounts Program, Canada (2024).
- CRCA Canadian Roofing Reference Manual: 7.1.3, membrane installation, 7.2.8, installation precautions and 13.2.4, thermoplastic membrane repairs (2020); CSA A123.21 application policy (November 2023).
- RCABC Roofing Practices Manual: TPO Roof Systems Standard (edition adopted January 20, 2026); UltraPly TPO acceptance.
- National Research Council Canada: A. Baskaran, S. Ko and F. Shyti, how to optimize wind resistance for low-slope membrane roofing systems (CRCA conference, 2023).
- Standards and Ontario rules: ASTM D6878/D6878M-26; CSA A123.21; CAN/ULC-S107; Ontario Fire Code, O. Reg. 213/07, 5.11 and 5.17; O. Reg. 213/91, ss. 1, 43, 52 and 195.2; Tremco TremPly TPO LV Bonding Adhesive safety data sheet (U.S. and Canada).
- U.S. sources: Johns Manville TPO Installation Guide and cold weather article (2019); Carlisle test welds and seam probing and inspection tips (2023); Versico seam probing (2019) and welding guidelines (2023); FRSA, common TPO welding problems (2021); Professional Roofing, Testing TPOs (2015); Facilitiesnet, roof failure: effect and cause (2003); BUILDINGS, TPO repair tips (2011); Colorado Roofing Association, understanding total system warranties (2021).
- OYH Roofing project records: Millomat Stampings, Mississauga; Devi Mandir, Pickering (October 2026).