OYH Roofing

Short answer

EPDM roof installation puts one sheet of synthetic rubber over insulation and holds it down with adhesive, fasteners in the seams, or stone ballast. Because EPDM cannot be melted, its seams are joined with primer and tape, not heat. Most EPDM roof repairs are peel-and-stick patches on cleaned, primed rubber, and asphalt roof cement must never touch it.

What is an EPDM roof?

EPDM (ethylene propylene diene terpolymer, the name used in its ASTM standard) is a synthetic rubber sheet, usually black and sometimes white, laid in one layer over the insulation. It is a thermoset, so unlike TPO and PVC it cannot be melted and welded: its seams are joined with primer and tape. The EPDM Roofing Association (ERA) says EPDM is made in North America by Carlisle, Elevate (formerly Firestone) and Johns Manville.

EPDM membrane options for commercial roofs. Sources: Carlisle Sure-Seal data sheet and EPDM Field Guide (July 2025, U.S.); Elevate Canada 25-year RubberGard warranty bulletin (November 2024) and RubberGard EPDM SA data sheet (March 2024, U.S.); EPDM Roofing Association; CRCA Canadian Roofing Reference Manual, 7.2 (2020). As of October 2026.
SheetThicknessWhere it is used
Non-reinforced black EPDM45, 60 or 90 mil (1.14, 1.52 or 2.29 mm)Adhered and ballasted roofs. Carlisle recommends at least 60 mil and uses 90 mil for its 30-year warranties
Reinforced EPDM45, 60 or 75 milNeeded for mechanically fastened roofs (Carlisle, CRCA)
White EPDMVaries by makerAdhered or mechanically attached, not ballasted (ERA). Elevate's Canadian 25-year warranty covers white EcoWhite only when adhered
Fleece-back EPDMVaries by makerSet in mopping-grade asphalt or low-rise foam adhesive (CRCA)
Self-adhered EPDM60 mil (Elevate RubberGard SA)Factory adhesive on the back; can go down at -7°C. Excluded from Elevate's Canadian 25-year warranty

For how EPDM compares with other membranes, see our TPO vs EPDM guide; this page covers the work itself.

How is an EPDM roof installed?

EPDM roof installation follows seven steps, to the maker's specification. Most figures below come from Carlisle's EPDM Field Guide for its approved applicators (U.S., July 2025) and the Canadian Roofing Contractors Association (CRCA) reference manual; other makers set their own rules.

7 best practices for EPDM roof installation, step by step. Sources: Carlisle EPDM Field Guide (July 2025) and EPDM specification (July 2026), U.S.; Elevate RubberGard EPDM SA data sheet (March 2024, U.S.); CRCA Canadian Roofing Reference Manual, 7.2 (2020). Steps vary with the system and the maker. As of October 2026.
StepWhat happensWhat makers and CRCA require
1. Design and warrantyMaker, sheet, attachment and warranty length chosenThe warranty sets thickness and detailing; Carlisle reviews ballasted roofs over 23 m (75 ft) high and freezer buildings
2. Deck, insulation, cover boardBoards fastened or glued to the deckCarlisle: polyiso to ASTM C1289 Type II, Class 1, Grade 2, and at least 5 fasteners per 1.2 x 2.4 m board under adhered sheet
3. Unroll and relaxThe sheet lies flat before it is attachedAbout 30 minutes (Carlisle, CRCA), longer in cold weather (Elevate)
4. Attach the sheetAdhesive, fasteners in the seams, or ballastCRCA: adhered rolls no wider than 3 m (10 ft); ballast placed as each section is finished (Carlisle)
5. Tape the seamsCleaned, primed and taped laps, rolled at onceLaps at least 63 mm (2 1/2 in) with 76 mm (3 in) tape; T-joints covered
6. Perimeter and flashingsBase of walls and curbs fastened, then flashedSecurement strips fastened every 300 mm (12 in) or less; flashings at least 200 mm (8 in) up the wall (CRCA)
7. Inspection and warrantyThe maker inspects before issuing a warrantyCarlisle's inspection "is not intended as a final inspection for the benefit of the owner"

Tear-off, daily seals and keeping a building open during the work are covered in our commercial roof replacement guide, and cover boards and vapour retarders in the TPO roof installation guide.

Fully adhered, mechanically fastened or ballasted?

All three are common, and self-adhered sheet is a fourth option. The deck, the building height, the wind load and the weight the structure can carry decide which. The ERA says ballasted roofs make up about 35 per cent of EPDM installations.

EPDM attachment methods. Sources: Carlisle EPDM Field Guide (July 2025) and specification (July 2026), U.S.; Elevate TIS 610 (March 2024, U.S.); EPDM Roofing Association; CRCA Canadian Roofing Reference Manual, 7.2 (2020). As of October 2026.
MethodHow the sheet is heldLimits and requirements
Fully adheredBonding adhesive rolled on the sheet and the board, flashed off until it no longer strings, then the sheet is folded in and broomed (Carlisle)No maximum slope (Carlisle). Carlisle limits its water-based adhesive to 20-year warranties and winds up to 72 mph (116 km/h)
Mechanically fastenedPlates or bars every 150 to 300 mm (6 to 12 in) along the seam, covered by 152 mm (6 in) tapeReinforced EPDM only. CRCA: fasteners at least 25 mm into wood or concrete, 19 mm through steel or wood panel decks
BallastedLoose-laid sheet held down by stone or pavers; edges and penetrations fastenedCarlisle: 38 mm (1 1/2 in) rounded gravel at no less than 49 kg/m² (10 lb/sq ft). CRCA: about 60 kg/m² of 19 to 38 mm river stone, on slopes under 4 per cent
Self-adheredFactory adhesive on the back of the sheet, rolled with a heavy rollerDown to -7°C and rising (Elevate RubberGard SA, Carlisle Sure-Seal SAT)

Ballast is heavy: Carlisle wants a deck that can carry 12 to 15 lb/sq ft (about 60 to 75 kg/m²) of it on top of the roof, so an engineer confirms the structure first. Whatever the method, the assembly must be wind-tested under CSA A123.21, which Ontario's Building Code points to; our TPO guide explains that test.

How are EPDM seams made?

With primer and tape, not heat. Every EPDM roof seam is a lap of two sheets joined with pressure-sensitive seam tape, and the bond depends on clean, primed rubber. Carlisle's field guide (U.S.) sets out the steps:

  • Clean. Sheet that has been exposed for weeks gets weathered membrane cleaner first.
  • Prime. A thin, even coat, left until it no longer transfers to a dry finger, but not allowed to over-dry; the tape goes on shortly after.
  • Tape width. For 10- to 25-year warranties, laps at least 63 mm (2 1/2 in) wide with 76 mm (3 in) tape. For 30 years, 152 mm (6 in) tape on a 138 mm lap, or 3 in tape with a 6 in strip over the whole seam.
  • Roll at once. A 50 mm hand roller with firm pressure, right after the release liner comes off, with 3 to 13 mm of tape showing past the top sheet.
  • T-joints. Where three sheets meet, a 152 x 152 mm (6 x 6 in) cover, plus a 305 x 305 mm (12 x 12 in) cover for 25- and 30-year warranties and all 90 mil sheet.
  • Lap sealant. A bead at tape overlaps, around T-joint covers and on cut edges of reinforced sheet, finished the same day.
  • Layout. Laps shingled so they do not face the flow of water, and no seams inside drain sumps.

Older EPDM roofs were seamed with liquid splice adhesive, and by the mid-1980s U.S. surveys showed those seams failing. In tests by the U.S. National Institute of Standards and Technology (NIST, 2005), tape seams lasted as long as adhesive seams or longer, and clean, primed rubber gave the longest life. Carlisle's current field guide uses tape only.

How are flashings and the perimeter finished?

The sheet is fastened at the base of every wall, curb and roof edge before it is flashed, so wind and shrinkage cannot pull it away; Carlisle also secures any inside slope change steeper than 2 in 12.

  • Securement strips. Carlisle's reinforced strip is 152 mm (6 in) wide with factory tape, fastened with plates no more than 300 mm (12 in) apart; nails are not accepted. The CRCA calls these strips "the most common approach for perimeter securement of EPDM".
  • Flashing height. At least 200 mm (8 in) up the wall and 75 mm (3 in) onto the roof (CRCA).
  • Termination bars. Carlisle's is a 25 mm aluminum bar punched every 152 mm and fastened straight to the wall; where metal counterflashing is added above, the bar is still the primary seal.
  • Uncured flashing. The stretchy uncured EPDM is kept for inside and outside corners, pipes, scuppers and odd shapes where moulded boots or cured sheet will not work (Carlisle).
  • Drains and pipes. The sheet runs 25 mm inside the drain clamping ring with sealant under it, never cut back to the bolts; pipes get moulded boots or field-made flashing at least 200 mm up the pipe (CRCA).

Curbs and units are covered in our rooftop equipment guide, and how details fail later in our roof flashing repair guide.

Can EPDM roof installation be done in winter?

Yes, with care. The rubber stays flexible far below Ontario lows: Carlisle rates its non-reinforced sheet brittle only at -45°C. The limits are the tape, primer and adhesives, which lose tack in the cold.

Cold-weather limits for EPDM products. Sources: Carlisle EPDM Field Guide (July 2025) and Aqua Base 120 data sheet (August 2022); Elevate TIS 817 and TIS 830 (September 2025) and TIS 610 (March 2024). All U.S. documents; Canadian data sheets may differ, and other makers set their own limits. As of October 2026.
Product or stepLimitWhat crews do
Seam tape and peel-and-stick partsLose tack below 4°C (Carlisle)Tape kept in heated boxes; primed sheet and tape warmed with a hot-air gun before rolling
Solvent bonding adhesiveAbove -6.7°C and rising (Elevate BA-2004)Stop near the dew point: evaporating solvent can leave condensation on fresh adhesive (Carlisle)
Water-based and solvent-free adhesives4°C and rising (Carlisle, Elevate)Elevate: not used if it will freeze within 12 hours
Self-adhered EPDM-7°C and rising (Elevate, Carlisle); 0°C for Carlisle's white SATRolled firmly; end laps stripped in
Relaxing the sheetAt least 30 minutesLonger in colder weather (Elevate)

So winter EPDM roof installation leans on solvent adhesives, fastened, ballasted or self-adhered sheet, and heated storage for the tape. Our flat roofing material guide compares cold ratings for every system.

What must never touch an EPDM roof?

Asphalt, oils and grease, above all. The CRCA manual says asphalt, coal tar, oil-based and plastic roof cements "are not to be used in direct contact with rubber-based components" of an EPDM roof, and lists petroleum products, greases, mineral and vegetable oils, animal fats and heat over 82°C (180°F) as things to keep away from it.

Materials to keep away from EPDM roofs. Sources: CRCA Canadian Roofing Reference Manual, 7.2 and 13.2.5 (2020); RCABC EPDM Roof Systems Standard, 9.1.3.4 (2026); U.S. Department of Veterans Affairs guide specification 07 53 23 (2021) and UFGS 07 53 23 (August 2025), U.S.; Carlisle EPDM specification (July 2026, U.S.). As of October 2026.
MaterialWhat the sources sayWhat is done about it
Old asphalt roof left in place (built-up or modified bitumen)EPDM must not be used over bituminous materials "where direct contact occurs" (VA, U.S.)A thin layer of insulation, a slip sheet or a separator sheet between the two (VA, U.S.)
Kitchen exhaust grease"Grease and oil attack EPDM" (UFGS, U.S.)A grease-resistant overlay in the exposure area (VA, U.S.); RCABC suggests other measures, including a liquid membrane. See our restaurant roofing guide
Asphalt roof cement, coal tar, oil-based and plastic cementsNot to touch the rubber (CRCA)Only the EPDM maker's own repair products
Petroleum products, equipment fluids, hot pipesOn RCABC's list of things membranes must be protected fromCarlisle reviews any roof exposed to petroleum, grease, oils or animal fats before the job

Water is not on the list: the ERA says ponded water "will not void a manufacturer's warranty", though each maker's own warranty is what counts. Our ponding water guide explains why drainage still matters.

What standards and Ontario rules apply to EPDM?

A U.S. product standard for the sheet, wind and fire tests for the assembly, and Ontario's workplace rules. These are the points specific to EPDM.

  • ASTM D4637. The specification for EPDM roofing sheet (D4637/D4637M-15, reapproved 2021), for non-reinforced, reinforced and fabric-backed sheet. Field seams, wind uplift and fire are left to the roof design; uncured flashing has its own standard, ASTM D4811.
  • No Canadian standard. We found no current CSA or CGSB standard for EPDM; the old CGSB elastomeric sheet standard (37-GP-52M, 1984) is listed as withdrawn, so Canadian specifications cite ASTM D4637.
  • A Canadian benchmark. B.C.'s RoofStar EPDM standard (January 20, 2026) asks for D4637 sheet, at least 60 mil on exposed roofs, the maker's own perimeter securement and a 2 per cent minimum slope on new roofs. It is a B.C. guarantee program, not an Ontario rule.
  • Wind and fire. CSA A123.21 for wind uplift and CAN/ULC-S107 for fire are rated by assembly, as on TPO; see our TPO standards section. Carlisle's ballast tables use ANSI/SPRI RP-4, a U.S. standard the Ontario Building Code does not name, so the engineer and the maker confirm ballast weights.
  • Solvent adhesives. A U.S. safety data sheet for a low-VOC EPDM bonding adhesive (GenFlex, 2023) classes it as a Category 2 flammable liquid with a flash point of -10°C, and calls for explosion-proof ventilation. Ontario's flammable liquid rules (O. Reg. 213/91) and exposure limits (Reg. 833) apply on site.
  • VOC limits. Canada's VOC Concentration Limits for Certain Products Regulations (2023) cap contact adhesives in containers under 3.785 L, such as small repair cans; we found no limit for roofing adhesive in pails.
  • Recycling. A tear-off recycling program reached parts of southern Canada around 2006 to 2011 (ERA); we found no current program for Ontario job sites.

Planning an EPDM roof?

We can check the deck and the old roof, set out the attachment method and details, and compare EPDM membrane and warranty options for your building.

Call 1-833-775-7663Request an assessment

What does EPDM roof repair involve?

Usually a peel-and-stick patch over cleaned, primed rubber. The ERA says EPDM is "typically repaired with pressure-sensitive (peel & stick) adhesive products" once the sheet is cleaned and primed, that the work needs no power or heat source, and that repairs can be made in extreme heat or cold.

  • Clean first. Tape will not stick to the dirty, weathered surface of old EPDM. Carlisle washes the area with a low-sudsing soap, rinses and dries it, then scrubs with weathered membrane cleaner or primer until the rubber is "a consistent matte black color without streaking".
  • Cuts, tears and punctures. A patch with rounded corners, so the corners cannot peel. Carlisle extends it at least 76 mm (3 in) past the damage; the CRCA asks for 75 mm with tape patches and 150 mm (6 in) with adhesive patches. Edges get lap sealant.
  • Open seams. The loose top layer is cut away, then the seam is cleaned, primed and covered with a strip at least 152 mm (6 in) wide centred over its edge (Carlisle). The CRCA adds a check for wet insulation before the seam is closed.
  • Loose fasteners. A new fastener beside the old one, patched 75 mm beyond (CRCA).
  • Shrunken or tired flashings. The ERA says service life can often be extended by adding new peel-and-stick flashings over the original ones, or after removing them. We found no maker procedure for the "bridging" that shrinkage causes at walls, so that repair follows the maker's own details.
  • What not to use. Asphalt, coal tar, oil-based and plastic roof cements (CRCA), and products from other makers, which Carlisle's warranty disclaims.

New EPDM can sometimes go over an old roof: the ERA says an existing roof "may be left in place once the manufacturer's substrate preparations are followed". RCABC calls recovering "not a recommended practice", allowed only by written variance and never over a roof already recovered, with the old sheet cut up, wet material removed and an insulation board fastened over it.

Old EPDM is often worth an EPDM roof repair. In research summarized by the ERA, samples from roofs in service 28 to 32 years still met new-sheet tensile and elongation minimums, with heat aging done at the National Research Council of Canada's Ottawa lab (2015). The ERA, an industry group, now puts expected service life at "at least 38 years", from a 2026 survey of roofing professionals. To weigh the options, see our repair or replace guide and our membrane roof repair guide.

How do you choose an EPDM roofing contractor?

Check the contractor's standing with the maker first, because it decides the warranty. Carlisle's warranties need a Carlisle Authorized Roofing Applicator, and Elevate's Canadian 25-year Red Shield warranty needs a licensed Elevate applicator. For WSIB clearance, insurance and other checks, see our guide to choosing a commercial roofing contractor.

Questions to ask an EPDM roofing contractor. Sources: Carlisle EPDM specification (July 2026) and warranty update (October 2024), U.S.; Elevate Canada RubberGard warranty bulletin (November 2024) and Platinum system page; Carlisle EPDM Field Guide (July 2025, U.S.). As of October 2026.
QuestionWhy it matters
Which maker, which sheet and what thickness?Elevate Canada's 25-year warranty needs at least 60 mil; its 30-year Platinum system uses 90 mil. Carlisle (U.S.) needs 90 mil for a 30-year adhered roof
Are you approved by that maker today?Without an authorized or licensed applicator, there is no system warranty
How wide is the seam tape, and how are T-joints covered?Longer warranties need 6 in tape or cover strips and larger T-joint covers; water-based adhesive caps Carlisle warranties at 20 years
What is your cold-weather plan?Below 4°C, tape needs heated storage and hot-air guns, or a self-adhered sheet
Which warranty terms apply in Canada?Carlisle's U.S. specification offers its Total System Warranty for buildings "within the United States", so get the Canadian terms in writing

The maker's inspection protects the maker's warranty, not necessarily the owner, so some owners also hire their own roof consultant. Our commercial roof warranty guide explains each warranty type.

Does OYH Roofing install EPDM roofs?

Yes. OYH Roofing handles EPDM roof installation and EPDM roof repair along with TPO, PVC, modified bitumen and built-up roofs on commercial, industrial and institutional buildings across Ontario. Our published projects so far are single-ply TPO roofs in Pickering and Mississauga, a PVC roof in Sault Ste. Marie and 2-ply modified bitumen roofs in Welland, Mississauga and Vaughan.

OYH Roofing logo on a crew member's hoodie during a winter roof job
An OYH Roofing crew member on a winter job. On any roof, EPDM included, the crew works to the maker's specification so the system warranty holds.

See our completed projects. To compare systems first, see TPO vs EPDM and our guide to the best flat roofing material for Ontario winters; for lifespans, see how long a commercial flat roof lasts.

Frequently asked questions

What is commercial rubber roofing called?

EPDM, short for ethylene propylene diene terpolymer: a synthetic rubber sheet, usually black, sometimes white, and commonly 45, 60 or 90 mil thick. On commercial buildings it is adhered, fastened or ballasted over insulation, and its seams are joined with primer and tape. TPO and PVC are sometimes called rubber roofs too, but they are plastics with heat-welded seams.

Do you glue down EPDM roofing?

Often, but not always. A fully adhered EPDM roof is glued to the insulation or cover board with bonding adhesive rolled onto both surfaces. EPDM can also be fastened through its seams with plates or bars, held down with stone ballast, or laid as self-adhered sheet with factory-applied adhesive. The deck, the wind load and the weight the structure can carry decide which.

How to join two pieces of EPDM?

With a taped seam. The lap is cleaned, primed with the maker's EPDM primer and left until it no longer transfers to a dry finger, then pressure-sensitive seam tape goes in and the seam is rolled at once. Carlisle uses 76 mm (3 in) tape for most warranties and 152 mm (6 in) tape for 30 years, with covers at T-joints and lap sealant at tape overlaps.

Can an EPDM roof be repaired?

Yes. Cuts, punctures, open seams and tired flashings are usually repaired with peel-and-stick EPDM patches and strips once the rubber is washed, cleaned and primed. Patches reach at least 75 mm (3 in) past the damage and have rounded corners. The EPDM Roofing Association says these repairs need no power or heat source and can be made in hot or cold weather.

Can you put new EPDM over old EPDM?

Sometimes. The EPDM Roofing Association says an old roof can stay in place if the maker's substrate preparation is followed and the roof and deck are inspected first. B.C.'s RoofStar program allows it only by written variance, never over a roof already recovered, with the old sheet cut up, wet material removed and an insulation board fastened on top. Ask the maker before planning it.

Can I install EPDM rubber roofing myself?

Not on a commercial roof if you want a maker's warranty. Carlisle and Elevate issue system warranties only on roofs installed by their authorized or licensed applicators, and the maker inspects the roof before issuing one. Commercial roof work also falls under Ontario's construction safety regulation, O. Reg. 213/91, including fall protection and the rules for flammable adhesives.

Need a roof that lasts?

Tell us about your building and roof, and we will set up a roof assessment and a written quote.

Call 1-833-775-7663Request an assessment
Karol Rajkowski, Vice President of OYH Roofing

Karol Rajkowski

Vice President · OYH Roofing

Karol Rajkowski is Vice President of OYH Roofing, an Oakville-based ICI flat-roofing contractor whose projects include the 6,500 sq ft TPO roof at Devi Mandir in Pickering and the 17,500 sq ft PVC roof on a new residential building in Sault Ste. Marie. Learn more about the OYH team.

Sources

OYH Roofing, 2120 Speers Rd, Oakville, ON L6L 2X8 · 1-833-775-7663 · info@oyhroofing.ca